<?xml version="1.0" encoding="UTF-8"?><?xml-stylesheet type="text/xsl" href="static/style.xsl"?><OAI-PMH xmlns="http://www.openarchives.org/OAI/2.0/" xmlns:xsi="http://www.w3.org/2001/XMLSchema-instance" xsi:schemaLocation="http://www.openarchives.org/OAI/2.0/ http://www.openarchives.org/OAI/2.0/OAI-PMH.xsd"><responseDate>2026-07-14T01:50:40Z</responseDate><request verb="GetRecord" identifier="oai:uvadoc.uva.es:10324/72884" metadataPrefix="etdms">https://uvadoc.uva.es/oai/request</request><GetRecord><record><header><identifier>oai:uvadoc.uva.es:10324/72884</identifier><datestamp>2025-03-26T19:10:02Z</datestamp><setSpec>com_10324_1157</setSpec><setSpec>com_10324_931</setSpec><setSpec>com_10324_894</setSpec><setSpec>col_10324_1298</setSpec></header><metadata><thesis xmlns="http://www.ndltd.org/standards/metadata/etdms/1.0/" xmlns:doc="http://www.lyncode.com/xoai" xmlns:xsi="http://www.w3.org/2001/XMLSchema-instance" xsi:schemaLocation="http://www.ndltd.org/standards/metadata/etdms/1.0/ http://www.ndltd.org/standards/metadata/etdms/1.0/etdms.xsd">
<title>Thin-Film Composite Cyclomatrix Poly(Phenoxy)Phosphazenes Membranes for Hot Hydrogen Separation</title>
<creator>Radmanesh, Farzaneh</creator>
<creator>Sudholter, Ernst J.R.</creator>
<creator>Elshof, Maria G.</creator>
<creator>Benes, Nieck E.</creator>
<description>Producción Científica</description>
<description>An interfacial polymerization process is introduced for the fabrication ofthermally stable cyclomatrix poly(phenoxy)phosphazenes thin-film com-posite membranes that can sieve hydrogen from hot gas mixtures. Byreplacing the conventionally used aqueous phase with dimethyl sulfoxide/potassium hydroxide, a variety of biphenol molecules are deprotonated toaryloxide anions that react with hexachlorocyclotriphosphazene dissolvedin cyclohexane to form a thin film of a highly cross-linked polymer film. Thefilm membranes have persistent permselectivities for hydrogen over nitrogen(16–27) and methane (14–30) while maintaining hydrogen permeances in theorder of (10−8–10−7 mol m−2s−1Pa−1) at temperatures as high as 260 °C anddo not lose their performance after exposure to 450 °C. The unprecedentedthermal stability of these polymer membranes opens the potential for indus-trial membrane gas separations at elevated temperatures.</description>
<date>2024-12-19</date>
<date>2024-12-19</date>
<date>2023</date>
<type>info:eu-repo/semantics/article</type>
<identifier>Adv. Mater. Interfaces 2023, 10, 2202077</identifier>
<identifier>https://uvadoc.uva.es/handle/10324/72884</identifier>
<identifier>10.1002/admi.202202077</identifier>
<language>eng</language>
<relation>https://onlinelibrary.wiley.com/doi/full/10.1002/admi.202202077</relation>
<rights>info:eu-repo/semantics/openAccess</rights>
<rights>http://creativecommons.org/licenses/by-nc-nd/4.0/</rights>
<rights>Attribution-NonCommercial-NoDerivatives 4.0 Internacional</rights>
</thesis></metadata></record></GetRecord></OAI-PMH>