• español
  • English
  • français
  • Deutsch
  • português (Brasil)
  • italiano
    • español
    • English
    • français
    • Deutsch
    • português (Brasil)
    • italiano
    • español
    • English
    • français
    • Deutsch
    • português (Brasil)
    • italiano
    JavaScript is disabled for your browser. Some features of this site may not work without it.

    Navegar

    Todo o repositórioComunidadesPor data do documentoAutoresAssuntosTítulos

    Minha conta

    Entrar

    Estatística

    Ver as estatísticas de uso

    Compartir

    Ver item 
    •   Página inicial
    • PRODUÇÃO CIENTÍFICA
    • Departamentos
    • Dpto. Física Aplicada
    • DEP31 - Artículos de revista
    • Ver item
    •   Página inicial
    • PRODUÇÃO CIENTÍFICA
    • Departamentos
    • Dpto. Física Aplicada
    • DEP31 - Artículos de revista
    • Ver item
    • español
    • English
    • français
    • Deutsch
    • português (Brasil)
    • italiano

    Exportar

    RISMendeleyRefworksZotero
    • edm
    • marc
    • xoai
    • qdc
    • ore
    • ese
    • dim
    • uketd_dc
    • oai_dc
    • etdms
    • rdf
    • mods
    • mets
    • didl
    • premis

    Citas

    Por favor, use este identificador para citar o enlazar este ítem:https://uvadoc.uva.es/handle/10324/72671

    Título
    Partially pyrolyzed membranes (PPMs) derived from copolyimides having carboxylic acid groups. Preparation and gas transport properties
    Autor
    Maya, Eva M.
    Tena Matias, AlbertoAutoridad UVA Orcid
    de Abajo, Javier
    de la Campa, Jose G.
    Lozano, Angel E.
    Año del Documento
    2009-12
    Editorial
    Elsevier
    Documento Fuente
    Journal of Membrane Science 349 (2010) 385–392
    Resumo
    A series of partially pyrolyzed membranes (PPMs) were prepared from a copolyimide having carboxylic acid pendant groups (PIA). The effect of the final pyrolysis temperature (425, 450 and 475 °C) on the gas separation properties was investigated and compared with those of PIA. The thermal treatments caused a progressive removal of the carboxylic acid pendant groups of PIA and a simultaneous increase of the fractional free volume of the PPMs. Thus, it was found that the permeability coefficients of PPMs were higher than that of PIA, between 6.5 and 25 times higher, depending on the gas tested and the final pyrolysis temperature, while the selectivity slightly decreased. All PPMs were attractive materials to separate CO2 from CH4 since were inside the commercially interesting region and are close to the present Robeson trade-off limit line. The pyrolysis at 475 °C yielded the PPM with the best performance: CO2/CH4 selectivity of 47 and CO2 permeability close to 95 barrers.
    Revisión por pares
    SI
    DOI
    10.1016/j.memsci.2009.12.001
    Patrocinador
    Spanish Ministerio de Ciencia e Innovación (project MAT-2007-62392)
    Version del Editor
    https://www.sciencedirect.com/science/article/pii/S0376738809008825
    Propietario de los Derechos
    elsevier
    Idioma
    eng
    URI
    https://uvadoc.uva.es/handle/10324/72671
    Tipo de versión
    info:eu-repo/semantics/submittedVersion
    Derechos
    openAccess
    Aparece en las colecciones
    • DEP31 - Artículos de revista [167]
    Mostrar registro completo
    Arquivos deste item
    Nombre:
    JMS 2009 maya version enviada.pdf
    Tamaño:
    556.3Kb
    Formato:
    Adobe PDF
    Thumbnail
    Visualizar/Abrir

    Universidad de Valladolid

    Powered by MIT's. DSpace software, Version 5.10